Skip to main content

Re: [MW:24544] PWHT of branch connections.//B31.3

Dear Sir,

Thank you for the replies.

The temperature gradient along the main pipe (Header) are managed by the coils and wool. why not it be considered with the same theory around the branch. That is the basis of my doubt.

We are following the code requirements. It is because of my academic interest I raised this question. 

Coiling of a 60" dia (for example) pipe for a branch weld of 3/4" dia, logically is not explainable.

Thanking you

Hareesh K V
+91-8547859202

On Mar 18, 2016 12:21 PM, "Prakash Gotimukul" <gprakash31@gmail.com> wrote:
>
> Codes are written after careful consideration. So it is good to argue but better to follow the code. If there is any other code with other options, that needs discussion. More over the thicker side is considered as main line and thinner side as branch line.
>
> Rgds
> Prakash Gotimukul
> ASME AIS, Technical Manager ASME/ISO/PED
>  gprakash31@gmail.com.
> Tel: +9714 2778511 Mob:+97152 979 5678
>
> On Fri, Mar 18, 2016 at 10:42 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
>>
>> that is the reason controlling theromocouples and monitoring thermocouples are recommended in D10.10 (amount of energy required to heat the branch small compared to run pipe), similar recommendations are provided in WRC 452.
>> concern could be distortion or induced stresses due to circular or spot heating
>>
>> On 18 March 2016 at 10:02, Hareesh K V <hareesh13h@gmail.com> wrote:
>>>
>>> Dear Sir,
>>>
>>> My doubt is, the width of the  band (HB or GCB) along the length of main pipe is on the logic of diminishing temperature and its metallurgical effects. Why not it is not considered to do the pwht of the branch in the vicinity area of branch/RF pad only by the same logic of HB and GCB near the weld area of RF pad/branch.( This will reduce the consumption of power, coiling time etc.)
>>>
>>> Thanking you
>>>
>>> Hareesh K V
>>>
>>> On Mar 18, 2016 9:52 AM, "Raghuram Bathula" <raghurambathula@gmail.com> wrote:
>>>>
>>>> Dear Hareesh
>>>>
>>>> Yes, it is. guidance for placement of thermocouples can be reffered to para 6.6.4 of AWS D10.10
>>>> control thermocouples  on larger pipe and monitoring thermocouples  on smaller branch connection
>>>>
>>>>
>>>> On 18 March 2016 at 06:03, Hareesh K V <hareesh13h@gmail.com> wrote:
>>>>>
>>>>> Dear Sir,
>>>>>
>>>>> As per ASME B31.3, for branch connections, PWHT is to be done for the entire circumference of main pipe. Is there any exceptions/code interpretations for that, in Carbon steel material or Alloy steel material (SA335 Gr P9,95)?
>>>>>
>>>>> For example: A 3/4" branch is done on the main pipe of 60" dia. As per the code requirement, the entire 60" dia is to be wrapped with coil and PWHT is to be done.
>>>>>
>>>>> Thanks in advance.
>>>>>
>>>>> Regards,
>>>>>
>>>>> Hareesh K V
>>>>> +91-8547859202
>>>>>
>>>>>
>>>> -- 
>>
>> --
>> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
>> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>> ---
>> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
>> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>> To post to this group, send email to materials-welding@googlegroups.com.
>> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubne%3Dx3MBfpy_emdCNwcfMw9qSMQoJ5GBc4jQui-crbojA%40mail.gmail.com.
>>
>> For more options, visit https://groups.google.com/d/optout.
>
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOUP4q%2BoDwu%3D24HDDSMWwDghTv2yiAp72b9UsfAiC-VrQ0tToA%40mail.gmail.com.
>
> For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAM3LgAVEveH-iSM1%3DZGaJOY0P3ET%2BWzd1KUjPudDp4UBOEO3Rw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...