Skip to main content

[MW:24485] RE: 24479] Inspection Certification EN10204 3.1 in China

Hi friend,

As per EN 10204, different designation of classes are their, -

Ex 3.2, it is demanding witness / validation by TPI/Owner is mandatory, in the same STD 2.1, 2.2 Designations are also available – which manufacturers will submit his test reports, complying to other supporting documents.

Hence you can convince to china manufacturers stating that "as per EN 10204 – Designating 2.1 or 2,2"

Also that the material / product is going out of china then the documentation shall also be in accordance to the recipient country standards, because end user requirements has to comply.

 

Equivalent ISO code is ISO 10474

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Farzad
Sent: Friday, March 11, 2016 12:06 AM
To: Materials & Welding
Subject: [MW:24479] Inspection Certification EN10204 3.1 in China

 

Dear Engineers,

Recently we have gone to a project with a Chinese EPC contractor for a petrochemical plant which most procurements will be done from China.

Now the issue is that we need that EN 10204 certification should be mentioned in all procedures and certifications should be arranged based on this EN STD. But suddenly contractor refused this clause with excuses that this STD is only for Europe and not applicable in China. They claim in case of insist many Chinese vendors may decline and delivery time and price also will be increased.

Please help how we can answer and convince them that this STD should be followed with all vendors including Chinese ones, we need scientific and logical explanation to convince them officially. Also I'm wondering if there are any equivalent standards of EN10204 in China that can be referred to it with peace of mind to force vendors for following?

Thanks in advance for your advices and comments...

 

Best Regards,

Farzad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c4293ab0-f13d-4100-aef4-9061e94b7816%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...