Skip to main content

[MW:24491] Re: 24479] Inspection Certification EN10204 3.1 in China

Hello Mr. Kumar,

With thanks, noted your comment but we need EN10204 type 3.1 certification. Does it have any meaning that Chinese vendors cant follow this STD? EPC Contractor claims many Chinese vendors cant follow it and will give up and for others will cause to worse delivery time and price. Its meaningless in my opinion and whats the procedure for vendors to get this certification approved if they don't have it yet? Generally do they need to be audited to get this certification by any specific organization or not, just they have to follow its rules?
thanks,
Farzad



On Friday, March 11, 2016 at 9:01:20 AM UTC+3:30, Lakshman Kumar wrote:

Hi friend,

As per EN 10204, different designation of classes are their, -

Ex 3.2, it is demanding witness / validation by TPI/Owner is mandatory, in the same STD 2.1, 2.2 Designations are also available – which manufacturers will submit his test reports, complying to other supporting documents.

Hence you can convince to china manufacturers stating that "as per EN 10204 – Designating 2.1 or 2,2"

Also that the material / product is going out of china then the documentation shall also be in accordance to the recipient country standards, because end user requirements has to comply.

 

Equivalent ISO code is ISO 10474

 

Thanks & Regards,

Lakshman Kumar B,

+91 9440031459.

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of Farzad
Sent: Friday, March 11, 2016 12:06 AM
To: Materials & Welding
Subject: [MW:24479] Inspection Certification EN10204 3.1 in China

 

Dear Engineers,

Recently we have gone to a project with a Chinese EPC contractor for a petrochemical plant which most procurements will be done from China.

Now the issue is that we need that EN 10204 certification should be mentioned in all procedures and certifications should be arranged based on this EN STD. But suddenly contractor refused this clause with excuses that this STD is only for Europe and not applicable in China. They claim in case of insist many Chinese vendors may decline and delivery time and price also will be increased.

Please help how we can answer and convince them that this STD should be followed with all vendors including Chinese ones, we need scientific and logical explanation to convince them officially. Also I'm wondering if there are any equivalent standards of EN10204 in China that can be referred to it with peace of mind to force vendors for following?

Thanks in advance for your advices and comments...

 

Best Regards,

Farzad

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c4293ab0-f13d-4100-aef4-9061e94b7816%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8fe88b53-0094-48d8-a0ce-3c9f18110390%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Re: [MW:14950] RE: 14919] Stress relieving Rejected for 5 min less soaking time.

Dear All, I have been a CONSULTANT FOR such problem & my personal opinion is expressed as follow. I fully agree with views expressed so far. But bag to differ that " Code is a law, with engineering judgments. Hence the inspector has the rights to declare that the original HT was inadequate." Inspectors & total industry must resist the "REJECTION" . We as intellectual & having seniority must become practical. How the code will revise???. ANS.: One is experiments (Pure research) & second is such chances that gives opportunity to experiment !!! _______________________________________________________________________________________________ My understanding is that it is P1 material. In that case every pass normalizes the immediate bottom pass. Hence code requirement for P1 FOR MANDATORY SR is 32 mm & above thickness. SOLUTION:  In any case 0. After SR=PWHT no PTC testing is required as per code--Unless for low temp. vessels. That means code ...