Re: [MW:24508] Procedure Qualifications as per API 1104

Dear Dhanush,

you need to qualify  a pqr for pipe grade X65 to X65  using a wps having E-6010 and E-7018 /16 electrode  with SMAW process since both pipe  and flanges are having similar mech. & chem. properties .
see the attachments.

his will meet all your requirements.

Dear experts ,please correct me ,If my recommendations need further fine tuning.

Regards,

JIJILAL K.M.
​QA/QC Manager,Jurong Engg. ltd.
Bangkok, Thailand​



On 12 March 2016 at 15:23, Lalu Rajendran <lalucpt@gmail.com> wrote:
Hi Dhanush,

As per API 1104, "A major change in joint design (e.g. from V groove to U groove) constitutes an essential variable"
You can use the same PQR (X65 to X65) with 75deg groove angle butt joint. But you must show the joint details in your wps (see below).



Experts, correct me if I am wrong.

regards,
LALU


On Fri, Mar 11, 2016 at 8:13 PM, DHANUSH PR <pr.dhanush@gmail.com> wrote:
Hi all welding experts

I have to qualify some procedures as per API 1104 and I have least knowledge about this specification.....

First I will detail my Product

1).I have Pipe( API 5L X65 MS) to be welded with a flange(ASTM A 694F65) 75deg groove angle butt joint( V groove 75 deg included angle)

2) SamePipe will be welded with a nozzle
(ASTM a694 F65) set on joint groove fillet weld.

As per API 1104 Clause 5.4.2.2 (c) for question no. 1, whether I have to make two pqr of F65 to F65 and X65 to X65 combinations with V groove 75 deg included angle??
 and
as per API 1104 Clause 5.4.2.3 for question no 2 both above PQR's will suffice the requirement of nozzle to pipe welding...??


Regards

Dhanush


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/fb33ec56-f706-43b0-a5cb-77b1b3c08859%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13tc4qQSo_q15zK%3DUvyxExYWNbFfuGcry6biwDrmX8-9sg%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHjKo1WAyrXkV3mH7ChD5eqmHAQ6Q%2BWOU1mES9sXjhGP9w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...