Re: [MW:13066] Welding of AISI 316L to A516 Gr B regarding

 
Also it needs PWHT, since it thickness is more than 19 mm (As per ASME)

 
T.Mahendran,
Tabouk - KSA,

 
--- On Sat, 11/26/11, george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com> wrote:

From: george.dilintas@gr.bureauveritas.com <george.dilintas@gr.bureauveritas.com>
Subject: Re: [MW:13063] Welding of AISI 316L to A516 Gr B regarding
To: "materials-welding" <materials-welding@googlegroups.com>
Date: Saturday, November 26, 2011, 1:08 PM

Just 309 is ok. 316 with carbon steel will give hot cracks because of low FN. You need a filler metal with much higher Cr and Ni content to avoid low FN
Best regards
Dr Georgios Dilintas
Authorized Nuclear Inspector
Authorized Inspector Supervisor
HBS Regional Technical Manager

  From: Eswaran samikannu [eswaranaws@yahoo.co.in]
  Sent: 26/11/2011 12:54 ZE5B
  To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
  Subject: [MW:13062] Welding of AISI 316L to A516 Gr B regarding


Good day to all,
Please refer the attachment  for joint configuration, I have to qualify the procedure for AISI 316L to A516 Gr B steel
Thickness of the job maximum 64 mm. I proposed to use 35 mm thickness plate for qualification.Code requirement ASME Sec IX
My plan as follows
1) Buttering the Bevel area of A516 Gr B material using E 309 consumables up to 3 to 5 mm
2) Machining of Bevel & PT (NDT) & Fit up
3) Welding of A516 Gr B to to AISI 316L using E316 consumables 

Kindly  advice me what preheat temperature  & Interpass temperature can maintained during welding, Any PWHT required or not,any other precautionary measures during welding & mechanical testing.
My client not specified anything. Please someone advice to me.
Thanks
Regards
E.Jegan  
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...