Skip to main content

[MW:13012] RE: 13011] RE: 13008] NACE requirement, does the WPS requirement HIC Test?

Hi,

 

Based on the process requirement, the Pipe is specified for NACE Certification, in addition HIC requirement is specified for pipes/ fitting that fabricated from welded plates, also we specified for HIC is not required for seamless pipe / fittings.

 

 

Now for joining two pipes / fittings together whether it is seamless or welded pipe or fittings (fabricated from plates), does the WPS qualification requires HIC Testing?

 

If yes, what is the HIC Testing Procedure & Acceptance Criteria.?

 

 

Case A

 

 

 

 

Case B

 

 

Case C

 

 

Case F

 

 

 

Case G

 

Case I

 

 

 

Regards

 

Siva

 

Asset Integrity

 

Operation Assurance


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Friday, November 18, 2011 12:06 PM
To: materials-welding@googlegroups.com
Cc: Sivaselvam Ponandrum
Subject: [MW:13011] RE: 13008] NACE requirement, does the WPS requirement HIC Test?

 

Hello,

 

Your query is too general. Can you specify what're the design requirements, wrt PH2S, PCO2, Temperature or any other design variable.

 

What's the material specification for pipes?

 

Appreciate your response.

 

Thanks.

 

Pradip Goswami,P.Eng.IWE

Welding & Metallurgical Specialist & Consultant

Ontario,Canada.

Email-pgoswami@sympatico.ca,

pgoswami@quickclic.net

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sivaselvam Ponandrum
Sent: Thursday, November 17, 2011 3:49 AM
To: materials-welding@googlegroups.com
Subject: [MW:13008] NACE requirement, does the WPS requirement HIC Test?
Importance: High

 

Dear All,

 

For welding carbon steel pipe with NACE requirement, does the WPS qualification requires HIC Test?

 

 

Regards

 

Siva

 

Asset Integrity

 

Operation Assurance

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...