Re: [MW:13102] QW-200.4

No need to combine two WPS if you don't want benefit thickness of BM, you can use more one WPS in a single joint,if your WPS is qualified for BM thickness..
 
Mhaskar Aly
 
 
 
 
-------Original Message-------
 
Date: 29/11/2011 11:27:06
Subject: Re: [MW:13084] QW-200.4
 
Dear Sir,
 
Thanks for reply, but apart from your expaination, please let me know can we combine two existing WPS of different processes (Say GTAW & SMAW) of less than 13 mm thk in a single production joint as per QW-200.1 (f) ?
On Sun, Nov 27, 2011 at 10:41 PM, Aly <mhaskar.aly@gmail.com> wrote:
Advantage of combining two processes:
 
Suppose u have two wps as below
 
1: WPS with GTAW with 13mm base plate thickness (Base metal Qualification range is 26mm max) 
 
2:WPS with SMAW with 20mm base plate thickness (Base metal Qualification range is 40mm max) 
 
If u combined these two WPS, the advantage you can get is u can weld GTAW process double the max thickness between two process ie  (2 x 20mm = 40mm) not upto 26mm only.
 
You can use more than one WPS in one single joint, just to increase base metal thickness qualification range one can combine two process as per QW-200.4(b).
 
You can create many WPS from one single PQR as needed.
 
Hope this is clear for you..
 
Mhaskar Aly
 
 
 
 
-------Original Message-------
 
Date: 18/11/2011 21:08:13
Subject: [MW:13020] QW-200.4
 

Dear experts....Can anyone provide some Section IX interpretations for clause no.QW-200.4 ?................Can anybody explain this clause better ?...........It clearly states that multiple wps of different processes can be combined together and we can make a single wps combining that processes...........and from one pqr combining different processes ,individual wps can be prepared for each process..............the root deposites clause of min 13 mm is an ALTERNATE requirement....is it really applicable in which situation ?...............

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards

Hiren Sevak
Surveyor
Bureau Veritas - Ahmedabad
207, Abhishree
Opp Star India Bazaar,
Satellite Road,
Ahmedabad-380015
Tel No. 079-26925491/92

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...