Skip to main content

Re: [MW:13010] Fillet weld size for Non-pressure part as per sec-VIII Div.2 edition 2010

Dear experts,

can anyone suggest me an weld edge preparation in option of fillet weld of T joint. Material detail.joint should be an equal strength of base metal. 

Horizontal plate thk : 100 

vertical plate thk : 70mm 

Material : SS304

Regards,
Vaibhav Joshi

On Sat, Nov 12, 2011 at 9:45 AM, Fitria Rahman <t.chintaqa@gmail.com> wrote:
Hi Jun
Before measuring the weld size, ensure that the fillet weld is not convex or concave. Dimension fillet welds depends on its weld symbol. See the mark on the left of the weld symbol (triangle). 'Z' is indicating leg length (Z 10 means 10 mm leg length). 'a' is indicating throat thickness (a 7 means 7 mm throat thickness).

Rgds

2011/11/11 Jr. Chiong <wichiong@yahoo.com>

Experts,

How to measure a FILLET WELD SIZE?

Eagerly need your valuable response.


Jun
QC Inspector


From: Alpesh Sakhreliya <alpeshsakhreliya@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 11 November 2011, 15:04:45
Subject: Re: [MW:12941] Fillet weld size for Non-pressure part as per sec-VIII Div.2 edition 2010

T X 0.7 = FILLET SIZE
T= MIN WALL THIK.

On Fri, Nov 11, 2011 at 4:37 PM, vaibhav Joshi <vnjoshi.leo@gmail.com> wrote:
Dear Experts, I need an advice on following mentioned case.

What should be the fillet size of stiffner attachment weld as per ASME sec-VIII Div-2 ? It is basically a rib welding on non-pressure part but still component is a loading member similar to rib welding in saddle supports.

Component : Rib welding to the support structure 

Material : SS304

Construction code : ASME sec-VIII Div.2

Mentioned the clause no. if possible.


Regards,
VJ
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Best Regards,
 
Alpesh Sakhreliya
Technical Services
Gujarat State Petronet Limited
Direct: +91 79 66701527
Mobile:+91 9898265772

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...