FW: [MW:13081] Type of steel as per chemical proterties

Dear,

Use latest equipment optical emission spectrograph, so u can all elements even lighter than sulpher. Match results with ASME II .

-----Original Message-----
From: Abdul Hafeez
Sent: 28/11/2011 10:38:28 am
Subject: RE: [MW:13077] Type of steel as per chemical proterties

use optical emission spectrgraph for PMI and compare results with ASME sec II Part A or B.

Regards,
Abdul Hafeez

-----Original Message-----
From: c.nopadon@vipco-thai.com
Sent: 27/11/2011 4:38:25 am
Subject: RE: [MW:13064] Type of steel as per chemical proterties

Normal PMI equipment like XRF spectrometer cannot identify C. From my
knowledge , it must be portable spectrometer or similar which will be more
expensive than normal PMI. If PMI is required for stainless of which carbon
content is the issue such as 347H , it is possible that the client will
require PMI result with carbon content.

Regards,

C.Nopadon

From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of pankaj abhang
Sent: Saturday, November 26, 2011 1:04 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:13061] Type of steel as per chemical proterties

Dear How you identified carbon in PMI?..........


Regards,
pankaj

On Fri, Nov 4, 2011 at 11:50 PM, meisam shokri arfaei
<meisamshokri@gmail.com> wrote:

Dear friend,

This material is something like CK30. But this kind of material is heat
treatable and you have to sure about this. It is recommended to have a
metallographic test on it for undrestanding such a heat treatment.

Regards

On Fri, Nov 4, 2011 at 1:22 PM, U WYNN-NAING <u.wynn-naing@total.com> wrote:

Dear Experts,

We did PMI test on one unknown machine bolt from crane boom rest and result
is as follow:

Can someone tell me how can we trace the steel grade base on this result.

Is there any software available?

Thanks and Rgds,

WN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding%2Bunsubscribe@googlegroups.com>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--

M. Shokri Arfaei

International Welding Engineer (IWE)

ASNT NDT Level III

ERI Metallurgy Lab. Manager

Tel: +98-21-66283696

Fax: +98-21-66283693

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
<mailto:materials-welding%2Bunsubscribe@googlegroups.com>
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...