RE: Re : [MW:27562] Welding S355 JR

It is not correct.

A qualification to group 1.1 (max. S275) do not qualify for group 1.2 (which includes the S355).
Please see ISO 15614-1, table 5, note a stating the following:

"Test piece materials in groups 1, 2, 3 and 11 qualify the equal or lover specified minimum yield strength steels".


Yours sincerely
Kristian Lund Jepsen


-----Original Message-----
From: 'Maghroud Moussa' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: 24. marts 2018 16:32
To: 'raouf <materials-welding@googlegroups.com>
Subject: Re: Re : [MW:27560] Welding S355 JR

Thanks Mr. Raouf for your response, but can you tel whow so, i mean which EN codes or standards gives this permission.


Thanks.

MAGHROUD Moussa
QC Manager.

Le 23 mars 2018 1:22 PM, 'raouf salhi' via Materials & Welding <materials-welding@googlegroups.com> a écrit :
>
> Yes you can
>
>
> SALHI Raouf
> QA/QC Engineer
>
>
> Tel: Morocco +212628979891
>       Tunisia +21621458258
>
> --------------------------------------------
> En date de : Ven 23.3.18, 'Maghroud Moussa' via Materials & Welding <materials-welding@googlegroups.com> a écrit :
>
> Objet: [MW:27542] Welding S355 JR
> À: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
> Date: Vendredi 23 mars 2018, 0h02
>
> Dear experts  Please can you help to tell
> me if a PQR made with S275JR ( Process is SMAW 111, E 7018)
> can supporte welding of S355JR according to EN normes.  Best regard  Provenance : Courrier
> pour Windows 10
>  
>
>
>
> --
>
> https://materials-welding.blogspot.com/
>
> https://www.linkedin.com/groups/122787
>
> ---
>
> You received this message because you are subscribed to the
> Google Groups "Materials & Welding" group.
>
> To unsubscribe from this group and stop receiving emails
> from it, send an email to materials-welding+unsubscribe@googlegroups.com.
>
> Visit this group at https://groups.google.com/group/materials-welding.
>
> For more options, visit https://groups.google.com/d/optout.
>
>
> --
> https://materials-welding.blogspot.com/
> https://www.linkedin.com/groups/122787
> ---
> You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
> Visit this group at https://groups.google.com/group/materials-welding.
> For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...