Hi Prasad,

I do not understand, why is it not retain properties after PWHT of F65 forgings?

Most of F60 or F65 materials are supplied in Q&T condition with tempering at 540 Deg. C as per ASTM A694, unless you specifically asked for tempering temperature of at or above 660 Deg. C since it has to be stress relieved at 650 Deg. C. Unless you specify in PO specification, vendor will not supply with above condition and hence you cannot stress relieve F65 materials with 650 Deg. C.

If F65 is delivered with tempering temperature of >660 Deg. C then obsoletely you can use it with stress relieving. All these conditions shall be included in the PO specification and it can be available in the market.

Regards,

L. Prabhu kumar
Ph. no. 9003010978/ +968 95202761


From: N VENKATESWARA PRASAD <weldengr.velosi@gmail.com>
Sent: Wed, 14 Mar 2018 19:22:18
To: materials-welding <materials-welding@googlegroups.com>
Subject: [MW:27517] ASTM A 694 F 65 FLANGES
 
Hi Experts,
 
We are using ASTM A 182 F 22 materials in sub sea  tree parts.  These forgings needs to be welded to ASTM A 694 F 65 pup pieces.  We need to do PWHT at 650 deg. C  for 6 hours.  The F 65 forgings can not retain the properties due to PWHT.  Hence we are doing buttering the F 22 and carrying out PWHT and then welding to F 65 forging with out PWHT.  
 
 I am looking for supplier who can provide the F 65 forgings which can retain its properties with PWHT.  It shall meet the the mechanical properties including hardness ( 250 Hv10)  in the as welded and PWHT condition also.  This will give more savings as we are avoiding buttering.
 
Please share if your have any details on it.
 
Regards
 
Prasad
 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...