Dear Ankur,
As Mr. Ramesh informed on the basis, i would like to give a simple example for easy understanding. 
Consider an organisation has performed a PQR with GTAW process on XX date for a GTAW WPS qualification. Later on YY date, another PQR performed by the same organisation for SMAW process for a SMAW WPS qualification.
Now the organisation would have 2 WPSs with individual process on each of the WPS. Now a new job has come, which demands the combination of Processes in one WPS. In this instance, the 2 PQRs can be combined together to make 1 WPS with both processes involved, provided that all the essential variables in the PQRs are within the limits as allowed by Section IX. This is one possible reason among many as such.

Regards
Anandh

On Thu, Mar 15, 2018 at 12:40 PM, Ramesh <rameshkannandevaraj@gmail.com> wrote:
Hi
 

how non-impact tested PQR ( your third PQR)  supported with impact tested WPS !!! any thickness limitation they mentioned in WPS??? Need more details on that... 


To utilize the advantage of clause in ASME Sec IX-QW- 200.2(f), Multiple WPSs With One PQR or Multiple PQRs With One WPS,  


Welding Engineer decides the best possible combinations of various PQRS by supporting in single WPS by considering production weldment requirements, design aspects like service condition, Design / operating temp etc.. 


​Other basic reasons like to combine processes like Root pass from one PQR & Rest from other PQRs etc. or to cover thickness ranges or use multiple consumables combination or additional positions etc.. etc.. in Single WPS 






On Wed, Mar 14, 2018 at 7:32 PM, 'Chetan Kapadia' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Ankur,

It is general guide line to reduce number of WPS / PQR & technically why increase qualification requirements beyond bare minimum.

Over a period of time & with great understanding even code has gone to the extent of recognising concept of sWPS to further reduce the burden of inventing the wheel again & again in advance fast moving technological life.

It is this technical philosophy that even the third test piece preserved by you shall be useful in an eventuallity as either
1. In case of major repair at site requiring one additional PWHT; The validation by additional PWHT & testing shall become best directional results before proceeding for repair.

OR

2. In future the same equipment under different design temperature can be tested even prior to accepting an order. That means further validation for different criteria (This type of research & its acceptance from welding, metallurgy & corrosion as well as life cycle of equipment can expand the horizen
& value addition to international community.

Hope explanation shall be open for new discussion. 

Thanks & Regards,
C.B.Kapadia,
9892633442

Sent from Yahoo Mail on Android

On Wed, 14 Mar 2018 at 7:17 pm, Ankur Pandey
Dear All,

I have a WPS(Impact tested) which is supported by 03 different PQR's. One of PQR is impact tested at -46° C, other at -29°C and third one is not tested for impact. I am not sure what could be the reason for combining these PQR's other than impact requirements.

Can someone give me general guidelines what are the usual reasons for use combination of PQR's in single WPS.

Regards,
Ankur Pandey.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

[MW:5202] RE: 5200] NDT after PWHT

------------------------------------- Interpretation:  I‑89‑14 Subject:         Section I (1986 Edition, 1987 Addenda), PW‑11,                  NDE Prior to PWHT Date Issued:     December 15, 1988 File:            BC88‑393   Question: Does PW‑11 require that NDE be performed on welds after they have been subjected to the postweld heat treatment required by PW‑39?   Reply: No, unless the conditions described in PW‑11.2.2 exist. ---------------------------------------------- Interpretation:  VIII-1-98-09 Subject:         Section VIII, Division 1 (1995 Edition, 1996 Addenda); NDE                 ...