Skip to main content

RE: [MW:15088] Acceptance criteria for Tungsten Inclusion in RT


I found the acceptance criteria for tungsten inclusion which is a rounded indication in Mandatory appendix 4 of ASME Sec. VIII Div.1.
I think Jatin didn't read my question properly as i had clearly mentioned that Construction code was Sec VIII Div.1
 
Regards
 
Prem Nautiyal
 

--- On Mon, 8/13/12, Jean Staton <Jean.Staton@metco-ndt.com> wrote:

From: Jean Staton <Jean.Staton@metco-ndt.com>
Subject: RE: [MW:15084] Acceptance criteria for Tungsten Inclusion in RT
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: Monday, August 13, 2012, 6:06 PM

Curious, first code reference was ASME VIII, DIV. 1 why did you reference ASME B 31.3?  I am unable to see any reference in ASME VIII that tells me to reference B31.3.  WHY would we go to a piping code when we are on a vessel code in the first place?

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jatin Dave
Sent: Saturday, August 11, 2012 7:48 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:15064] Acceptance criteria for Tungsten Inclusion in RT

 

 

Dear Prem,

 

IN ASME B 31.3 Table No. 341.3.2 criteria are  given

 

F    Slag inclusion, tungsten inclusion, or elongated indication
                                             Individual length ≤ T w /3
                                             Individual width ≤ 2.5 mm (3⁄32 in.) and ≤ T w /3
                                             Cumulative length ≤ T w in any 12T w weld length
G           Slag inclusion, tungsten inclusion, or elongated indication
                                              Individual length ≤ 2T w
                                               Individual width ≤ 3 mm (1⁄8 in.) and ≤ T w /2
                                                Cumulative length ≤ 4T w in any 150 mm (6 in.) weld length

Please see Table 

 

Regards

Jatin Dave

9099026886

 


From: joydev dalai <joykolkata07@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 10 August 2012 10:51 AM
Subject: Re: [MW:15053] Acceptance criteria for Tungsten Inclusion in RT

 

Dear Prem,

 

There is nothing cleared about tungsten inclusion, for better information please see in ASME sec.VIII Div.1 ,UW-51 paragraph 

On Thu, Aug 9, 2012 at 9:24 PM, prem nautiyal <prem_nautiyal26@yahoo.com> wrote:

Dear Friends

 

After reviewing a RT film of a Circ.seam joint (16mm thk), which has been welded with TIG + SMAW, i have observed a tungsten inclusion @2-3mm in dia.

The construction code of the vessel is ASME Sec VIII Div.1

 

No doubt this tungsten inclusion is a defect, but i would like to know whether there is any acceptance criteria related to diameter for the same in ASME Sec VIII Div.1. Please give Code reference.

 

Regards

 

Prem Nautiyal

Cell: 9769316004

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 


DISCLAIMER: The information contained in this e-mail may be confidential and is intended solely for the use of the named addressee. Access, copying or re-use of the e-mail or any information contained therein by any other person is not authorized. If you are not the intended recipient please notify us immediately by returning the e-mail to the originator.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...