Skip to main content

Re: Re: [MW:28107] FABRICATION TRAVELLAR FORMATE (FOR HEAT EXCHANGER OR PRESSURE VESSEL)

ITP is being prepared based on process proposed sequence. In Traveller, production people is also taking responsibility by signature

On Mon, 23 Jul 2018 8:12 am Nithin Joseph, <nithindsilva4u@gmail.com> wrote:
Hi traveller is nothing but ITP. So no point in maintaining 2 documents.

On Sun, Jul 22, 2018 at 8:46 AM, Jay Poojary <jayogini@gmail.com> wrote:
Mr Jay Prajapati, 

This are not code requirements, this seems to be specific client requirements. Similar of this type we have for our orpic projects which is called Readiness program. 



On Sun, Jul 22, 2018, 8:37 AM jay prajapati <jay0000.jp@gmail.com> wrote:
Thanks dear,

Reference to trailing mail,
But i have also one formate which is different from ITP. which is given in detailed,(find attached file)

Now my question is.
Is ITP and traveler both are same things or different? 
If there is any other formate like this( attachment) then please provide, so i can make traveler in details by examine one or more.

On Sat, Jul 21, 2018 at 10:10 AM 'Shashank Vagal' via Materials & Welding <materials-welding@googlegroups.com> wrote:
You can always make it from an ITP.

Best Regards,

Shashank C Vagal (Quality Adviser), (+91) 8082395502, 8779046302,

NEO METAL-ANALYST & NDT SERVICES

·       A-25, Geet Siddhi, Boradevadi, Moshi-Haveli, PCMC, Pune 412105

·      301, PRATHAMESH, M G Rd – Mahant Rd, Vile Parle East, Mumbai 400 057 INDIA

www.neometalanalystndt.com / enquiry@neometalanalystndt.com / nach_sam@yahoo.com




On Friday, 20 July, 2018, 5:49:58 PM IST, muneebslsa@gmail.com <muneebslsa@gmail.com> wrote:


FYI



____________ 

Thanks & Regards,

MOHAMED          MUNEEB           MAHABOOB

JAPID

JAZAN-IGCC-001

M:                         +966(0)59 607 2237

O.E:     mahaboob.muneed@aramco.com

P.E:                  muneebslsa@gmail.com

 
Date: 2018-07-19 14:44
Subject: Re: [MW:28095] FABRICATION TRAVELLAR FORMATE (FOR HEAT EXCHANGER OR PRESSURE VESSEL)
fyi pl (Traveller)

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Thu, Jul 19, 2018 at 1:39 PM, JAY <jay0000.jp@gmail.com> wrote:
Dear professional, 


I just had my customer come see my shop and they asked me if I use 
shop travelers. I had to tell them no because I don't right now. I want to start using one but am having trouble finding a template online. Does anybody have a template, or a copy of one that I can use to make one?

Please Do the needful.

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Regards,
Dsilva

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...