Re: [MW:28036] MIC CORROSION or co2 wet corrosion(sweet corrosion)

Thank you so much for useful information.
Therefore you agree with me that these tests are not enough to conclude for SRB test.
Regardless of mentioned test, do you prescribe any other tests to consider possibility of co2 corrosion(mesa corrosion) or h2s pitting corrosion?

Regards.

On Wed, Jul 4, 2018 at 8:32 AM, 'Muhammad Hussain' via Materials & Welding <materials-welding@googlegroups.com> wrote:
This is not the method to measure SRB. There is a separate method called MSL for this and it's long time study, min 6 months to measure the SRB and it's status either it's living, present or absent. By then you can take a decision and precaution for eliminating this. 

Sent from my iPhone, Excuse Typos

On 4 Jul 2018, at 13:37, Ali Asghari <asgharialigl@gmail.com> wrote:

Unfortunately not.
I have attached them. I think this type of SRB test is qualitive.


On Tue, Jul 3, 2018 at 3:08 PM, 'Muhammad Hussain' via Materials & Welding <materials-welding@googlegroups.com> wrote:
It depends what is the current status of corrosion and how much damage is there? Also whats the materials of construction? 

Did your lab manage to measure the SRB and how much microbe is there? Without knowing this, its very hard to say what the material condition and how much time it will take to effect the material. 

Also depends on the MIC status as well. 





On Tuesday, July 3, 2018, 8:13:37 PM GMT+10, Ali Asghari <asgharialigl@gmail.com> wrote:


Dear Muhammad.
I have attached them.
I am only wondering that this corrosion with this rate may happen with detachable corrosion products by wetty co2 or h2s that affected by flow velocity.now how can we reach to this confidence or these results refuse this possibility.
Regards.
On Tue, Jul 3, 2018 at 7:03 AM, 'Muhammad Hussain' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear Ali, 

1. Yes it's possible and you can take. Corrosion deposit , metal or perhaps in water to do the analysis. 

2. Can you send clear images of the sample, specially from pits. 

Chloride and Sulphide are different source and affect on MIC. 

Regards 
Muhammad 

Sent from my iPhone, Excuse Typos

On 2 Jul 2018, at 23:04, Ali Asghari <asgharialigl@gmail.com> wrote:

Dear All.

We encountered to a pitting corrosion that led to loss of fluid in crude pipeline, so we prepared a sample and send it to lab.it must be mentioned that this corrosion happened after 6 

months from starting of production and there is possibility for existence of remained hydro test water and the chemical injection not to start any inhibitor injection with regarding in 
engineering design documents, availability of 95% inhibitor requested and warned for retained water to increase of pitting opportunity.

the lab concluded the result of this corrosion is MIC(SRB type) with doing of these tests: EDS/XRD/SRB test.
Now I have some doubts:
1.SRB or anaerobe bacteria can be survived & detected in air to reach Lab.

2.I know that to get conclusion by now is not possible but I want to know that are these tests enough or what is supposed to be done other tests to refuse co2 corrosion?

I have attached some results.

Regards.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
<20180702_164353.jpg>
<20180702_164522.jpg>
<20180702_164557.jpg>
<20180702_164704.jpg>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3fh9Rvt0j2E/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3fh9Rvt0j2E/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
<Untitled.jpg>

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to a topic in the Google Groups "Materials & Welding" group.
To unsubscribe from this topic, visit https://groups.google.com/d/topic/materials-welding/3fh9Rvt0j2E/unsubscribe.
To unsubscribe from this group and all its topics, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Re: [MW:34105] SA266 GR4N 4 Cycle SPWHT

Hi,  You are correct, Minimum refers to the one cycle for which this part will expose until final work shop PWHT. hence mill test certificate shall include this.  Max. SPWHT, refers to additional cycles of heat treatment that are reserved for future repairs during equipment lifetime.  Again, these simulated no. Of cycles shall be specified in MTC.  The idea is we need to make sure that steel mechanical properties are not compromised upon exposure to multiple repairs (i e 4 cycles in your case).  One could say, if steel is subjected to 4 cycles and is ok, then it should by defacto be good for one cycle, yet, this is wrong assumption cause mechanical problems and microstructure of materials varies accordingly based on no. Of cycles for which material will expose. This is apparent in alloy steel and especially for impact test values as an example.  In your case, this forged CS with properties before PWHT can be understood to be " as forged" condition (i.e. Wit...

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...