Skip to main content

Re: [MW:28049] RE: 28045] Enquiry about lower shell MPI while replacing Annular Plate in storage tank

Hi Dear ,


Annular plate have the inspection for first root DPT ,final UT,  then shell to annular plate diesel chalk test,VBT, outside .MPI OR LPT


REGARDS,

KISHOR
WELDING INSPECTOR 

TARIQ ALGHANIM 

On Tue, Jul 10, 2018, 6:56 AM tahir alam <tahiralam007@gmail.com> wrote:
We are following API 653 ,just wanted to know is it mention in code which test is required to check shell surface defect while replacing annular plate. Here two refinery one refinery is accepting MPI and other refinery not accepting MPI ,they told us to do LPT of shell.


Best Regards
Tahir Alam
Planning Engineer
Agam Tank Maintenance Group
Mobile : +(965)5150-1509


--------------------------------------------------------------------------------
Site Office : +(965)2388-3614
Head Office : +(965) 2398-5381l2
Fax : +(965) 2398-8312
P.O.Box : 9390 Ahmadi, 61004 Kuwait
Email : tahiralam007@gmail.com
Website : www.agamltd.com
-------------------------------------------------------------

On Tue, Jul 10, 2018 at 6:40 AM, PGoswami <pgoswami@quickclic.net> wrote:

What's the design code? Is there any additional requirement such as clients' specifications.

MPI & LPI are often interchangeable for determination of surface defects.

 

Thanks.

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of tahir alam
Sent: July 9, 2018 11:21 PM
To: materials-welding@googlegroups.com
Subject: [MW:28045] Enquiry about lower shell MPI while replacing Annular Plate in storage tank

 

Dear experts 

 

We have contract of tank maintenance in Kuwait. While replacing annular plate inspection ask to do DPT of 2 inch of shell plates. In another refinery they are agree to do MPI only while replacing the annular plates. kindly guide me which one is mention in code. If specifically mention in code then pls send me code detail also.


Best Regards

Tahir Alam

Planning Engineer
Agam Tank Maintenance Group
Mobile : +(965)5150-1509


--------------------------------------------------------------------------------

Site Office : +(965)2388-3614
Head Office : +(965) 2398-5381l2
Fax : +(965) 2398-8312
P.O.Box : 9390 Ahmadi, 61004 Kuwait
Email : tahiralam007@gmail.com
Website :
www.agamltd.com

-------------------------------------------------------------

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...