Re: [MW:28151] PIPELINE PQR /WPS API 5L Grade X60

Hi Sanjeev

Noted. 
7.2.1 has been modified as above in 2013 edition. i was referring 2012 edition. 

Next revision they mentioned july 2018. 

Thanks



On Mon, Jul 30, 2018 at 10:16 AM, Sajeev P <sajeevlaxmi@gmail.com> wrote:
Hi

I agree with Mr. Rameshkannan Devaraj except for Answer for question 1. As per the latest revisions ( 2013, 2016 and 2018) Para 7.2.1 states that " Welding procedures for pipelines designed to ASME B 31.4 or ASME B 31.8 shall be qualified with API STD 1104 or ASME SEC IX". Please refer your project standard cut off date.

Regards,
Sajeev


On Tue 24 Jul, 2018, 14:47 Ramesh, <rameshkannandevaraj@gmail.com> wrote:
Hi

My response for your query as below

1)  Pl refer Clause 7.2.1 of SAES-W-012, "All welding procedures for pipelines shall be qualified in accordance with API STD 1104 as required by the design codes, ASME B31.4 and ASME B31.8. 
     For other applications permitted by the design code, procedures may be qualified in accordance with ASME SEC IX."
2)  Pl refer Clause 7.4.19 & 7.2.1 Para 2 of SAES-W-012, - Required
3) & 4 )  Pl refer Clause 6.1.5 of SAES-W-012, go with manufacturer recommendation, Aramco is requirement is as per ASME Sec II C 
5)   Pl refer Clause 7.5.1 & 7.2.1 Para 2 of SAES-W-012, - Required
6)   Pl refer Clause 7.4 – Procedure Variable of SAES-W-012


Thanks and Regards


Rameshkannan Devaraj

"What you have learned is a mere handful; What you haven't learned is the size of the world – Avvaiyar"


On Mon, Jul 23, 2018 at 7:42 PM, Jay Jay <jaffarja1@gmail.com> wrote:
Dear Experts,

Need your suggestions/feedback for developing PQR /WPS for the following:-

Wet crude Sour service pipeline , ASME B31.4/31.8 , API 5 L Gr X60 ,ISO 15156 ,PSL2 , 24" ,12.7MM thickness, ASME Sec IX/API 1104 , Temperature range 0 to 90' C

My quarry:-

1)As per the applicable Aramco Standard ( SAES-W-012) , for Manual Welding process PQR can be qualified to either ASME SEC IX or API 1104, but many are insisting to use API 1104 to qualify as it is a pipeline . So kindly advise

2) Impact test required?

3)Suggested Welding Consumables for a) SMAW only b) GTAW & SMAW

4)Contractor is insisting for all pass Downhill welding using cellulosic electode E7010 for all passes,to avoid baking and storage requirements of Low hydrogen electrode(E7018).Is it possible ?

5)Hardness required for PQR?

6)Can this PQR be used for welding API 5L Grade B joints, without re-qualification?

Apologize for the lenghty quarry, waiting your valuable reponses.

Thank you 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...