The following is the text of ASME Section V , Article 7 
T-762 Lifting Power of Yokes
(a) Prior to use, the magnetizing power of electromagnetic
yokes shall have been checked within the past year.
The magnetizing power of permanent magnetic yokes shall
be checked daily prior to use. The magnetizing power of
all yokes shall be checked whenever the yoke has been
damaged or repaired.

(b) Each alternating current electromagnetic yoke shall
have a lifting power of at least 10 lb (4.5 kg) at the maximum
pole spacing
that will be used.

(c) Each direct current or permanent magnetic yoke
shall have a lifting power of at least 40 lb (18 kg) at the
maximum pole spacing
that will be used.

(d) Each weight shall be weighed with a scale from a
reputable manufacturer and stenciled with the applicable
nominal weight prior to first use
. A weight need only be
verified again if damaged in a manner that could have
caused potential loss of material.

Hence, No need for a third party certificate for the calibration and it OK if it has the manufactures certificate showing the weight lifting capacity and other test results

arun


On Mon, Apr 19, 2010 at 12:35 PM, Nishad AK <nishadamk@gmail.com> wrote:
Good day,
 
I have a query regarding the calibartion of MPI yoke both Electomagnetic & permanent magnetic type.
Does that should hold a Valid calibration certificate by the Third party calibration body or is that ok it has the manufactures certificate showing the weight lifting capacity and other test results.

--
Thanks and Regards

Nishad AK
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ARUNACHALAM.A
050-5257122

IT'S BETTER TO LOSE YOUR EGO TO THE ONE YOU LOVE.
THAN TO LOSE THE ONE YOU LOVE ....... BECAUSE OF EGO

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...