Skip to main content

Re: [MW:4941] Calibration of MPI yoke and validity.

Hello Mr. Andrew

Here is what I mean from ASME SEC V T-762 Lifting Power of Yokes (MR. Arunachalam A, already provide the exact wording of code what I am trying to say)

So I again repeat no third part calibration certificate required for the weight of calibration only the weight used for calibration must be from reputable manufacture. Unless it is specific requirement from client, seeking the calibration certificate from third party is wasting of money and time.

 (d) Each weight shall be weighed with a scale from a reputable manufacturer and stenciled with the applicable nominal weight prior to first use. A weight need only be verified again if damaged in a manner that could have caused potential loss of material.



On Fri, Apr 23, 2010 at 3:28 PM, Shashank Vagal <nach_sam@yahoo.com> wrote:
The gimmick here is what exactly to take for a "reputable manufacturer" of (weights and) scales and what would be the acceptable scale to weigh and confirm weight. What accuracy is allowed in weighing? The same weight measured by 2 or 3 scales of the same reputed manufacturer can vary. Then what?
As we do, we check the magnetizing power to detect certain depth defects in a mock up; while the stated ASME rulings are observed as a routine guideline.
Even a coil's performance depends a lot on how it is stored, one year is a long enough time when it can deteriorate and won't be as functional as in the beginning.
Just some cautious soundings............

--- On Fri, 23/4/10, Arunachalam A <arunvani@gmail.com> wrote:

From: Arunachalam A <arunvani@gmail.com>
Subject: Re: [MW:4936] Calibration of MPI yoke and validity. Date: Friday, 23 April, 2010, 10:15 AM


The following is the text of ASME Section V , Article 7 
T-762 Lifting Power of Yokes
(a) Prior to use, the magnetizing power of electromagnetic
yokes shall have been checked within the past year.
The magnetizing power of permanent magnetic yokes shall
be checked daily prior to use. The magnetizing power of
all yokes shall be checked whenever the yoke has been
damaged or repaired.

(b) Each alternating current electromagnetic yoke shall
have a lifting power of at least 10 lb (4.5 kg) at the maximum
pole spacing
that will be used.

(c) Each direct current or permanent magnetic yoke
shall have a lifting power of at least 40 lb (18 kg) at the
maximum pole spacing
that will be used.

(d) Each weight shall be weighed with a scale from a
reputable manufacturer and stenciled with the applicable
nominal weight prior to first use
. A weight need only be
verified again if damaged in a manner that could have
caused potential loss of material.

Hence, No need for a third party certificate for the calibration and it OK if it has the manufactures certificate showing the weight lifting capacity and other test results

arun


On Mon, Apr 19, 2010 at 12:35 PM, Nishad AK <nishadamk@gmail.com> wrote:
Good day,
 
I have a query regarding the calibartion of MPI yoke both Electomagnetic & permanent magnetic type.
Does that should hold a Valid calibration certificate by the Third party calibration body or is that ok it has the manufactures certificate showing the weight lifting capacity and other test results.

--
Thanks and Regards

Nishad AK
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ARUNACHALAM.A
050-5257122

IT'S BETTER TO LOSE YOUR EGO TO THE ONE YOU LOVE.
THAN TO LOSE THE ONE YOU LOVE ....... BECAUSE OF EGO
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
ą¤§ą¤Øą„ą¤Æą¤µą¤¾ą¤¦,
ą¤­ą¤¾ą¤øą„ą¤•ą¤° ą¤®ą¤Øą„‹ą¤¹ą¤° ą¤•ą¤¾ą¤³ą„‡
+60149129098

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...