Skip to main content

Re: [MW:4874] std & non standard range


<Security Level 2>                                                                                                                                                                                                                                                                                                                                                                                                                                
That depends on flange standard one is referring to.

However, most commonly followed are :
  • ASME B 16.5 : UP TO SIZE NPS 24
  • ASME B16.47 SR.A / SR.B : UP TO SIZE NPS 60 (for rating150& 300)
  • AWWA C-207 : UP TO SIZE NPS 144 (without Hub) & UP TO SIZE NPS 96 (With Hub) - Pls. refer this standard while giving reference of this for any size.

Thanks & Regards,
Dhwani Desai.
TOYO - PLANNING & PIPING DEPT.
91-22-2573 7681.



Yadav Shiva <luvshiv2002@gmail.com>
Sent by: materials-welding@googlegroups.com

04/19/2010 05:10 PM

Please respond to
materials-welding@googlegroups.com

To
materials-welding@googlegroups.com
cc
Subject
Re: [MW:4873] std & non standard range





Mr Noushad ,
                    These are very straight forward question,
1) What is the pipe size range  in which all flanges are standard ?
2) What is the pipe size range  in which all flanges are non standard ?

Can anybody help me out from this.

On Mon, Apr 19, 2010 at 11:57 AM, Noushad cp <ncp.clt@gmail.com> wrote:
Dear Mr.Shiva,
 
 
Pls Expalian the question in Detail way.
 
 
Noushad


 

On 4/19/10, Yadav Shiva <luvshiv2002@gmail.com> wrote:

What is the pipe size range  in which all flanges are standard & non standard?


--
Yadav Shiva Chelliya,
Inspection Engineer,
Doha Qatar,
+974-6166465
 

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to
materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.




--
Yadav Shiva Chelliya,
Inspection Engineer,
Doha Qatar,
+974-6166465

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...