Re: [MW:4897] Calibration of MPI yoke and validity.

Dear comrades,
 
IT Would great if anyone could suggest the appropriate ASTM std for the procedure on calibration of the MPI Yoke.

On Tue, Apr 20, 2010 at 12:09 PM, Kale, Bhaskar M <bmkale@gmail.com> wrote:
Weighing of calibration block /daily lift check  block required to do
with the weigh scale (weight measuring equipment) from the reputed
manufacturer. No calibration certificate of calibration block required
unless any client have the specific requirement. If any one asking  to
do the calibration from third party its just wasting of time and
money.
Regards, Bhaskar

On 4/20/10, SENTHILKUMAR SWAMINATHAN <skumarswami@yahoo.co.in> wrote:
> In my Org we are doing in house calibrationwith written procedure, but
> lifting block weight is certified by third party.
>
> Regards,
> S.Senthilkumar
>
> --- On Mon, 19/4/10, Nishad AK <nishadamk@gmail.com> wrote:
>
>
> From: Nishad AK <nishadamk@gmail.com>
> Subject: Re: [MW:4871] Calibration of MPI yoke and validity.
> To: materials-welding@googlegroups.com
> Date: Monday, 19 April, 2010, 2:37 PM
>
>
>
>
> My question is on validity of the MPI instument say for the
> purpose of project is valid only if that posess a Calibration certificate by
> a TP agency.or otherwise is acceptable.
>
> On Mon, Apr 19, 2010 at 12:54 PM, Bathula Raghuram (Mumbai - PIPING)
> <R.Bathula@ticb.com> wrote:
>
>
>
> In house is acceptable with a written calibration procedure. Permanent
> magnet type shall be calibrated ( check magnetic power) prior to use on
> daily base, and electromagnetic type on yearly basis.
>
>
>
> From: materials-welding@googlegroups.com
> [mailto:materials-welding@googlegroups.com] On Behalf Of Nishad AK
> Sent: Monday, April 19, 2010 2:06 PM
> To: materials-welding@googlegroups.com
> Subject: [MW:4868] Calibration of MPI yoke and validity.
>
>
>
>
>
>
>
> Good day,
>
> I have a query regarding the calibartion of MPI yoke both Electomagnetic &
> permanent magnetic type.
> Does that should hold a Valid calibration certificate by the Third party
> calibration body or is that ok it has the manufactures certificate showing
> the weight lifting capacity and other test results.
>
> --
> Thanks and Regards
>
> Nishad AK
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
>
> --
> Thanks and Regards
>
> Nishad AK
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>
> Subscription settings:
> http://groups.google.com/group/materials-welding/subscribe?hl=en
>


--
धन्यवाद,
भास्कर मनोहर काळे
+60149129098

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks and Regards

Nishad AK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...