Skip to main content

RE: [MW:4909] RE: 4421] Hispeed fluxes for SAW WELDING

For wind tower production Oerlikon has specially designed OP 139

 

With kind regards,

Erwin GERING

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens hakan sitem
Verzonden: dinsdag 20 april 2010 23:08
Aan: materials-welding@googlegroups.com
Onderwerp: Re: [MW:4908] RE: 4421] Hispeed fluxes for SAW WELDING

 

Regarding to SAW using during wind tower production, you can try Esab OK 1072 flux combination together with your wires which is already presented to be used in wind tower production.

Bu e-posta, Turkcell BlackBerry ile gönderilmiştir.


From: bcube bcube <bcubebcube@gmail.com>

Date: Tue, 20 Apr 2010 20:53:36 +0530

To: <materials-welding@googlegroups.com>

Subject: Re: [MW:4901] RE: 4421] Hispeed fluxes for SAW WELDING

 

Dear gary,

 

now we are using the Lincoln Electric P223 flux , to weld the wind mill towers , but during welding we experience the following

1. uneven weld bead

2.excess reinforcement

3.bad cosmetic look

 

if decrease the amps to get good cosmetic look , during ut inspection the weld soundness fails. can you recommend a parameter for welding

 

Note:

 

the thickness range is 8mm to 20mm , we are practising square but welding .


 

On 3/5/10, Gary_Konarska@lincolnelectric.com.sg <Gary_Konarska@lincolnelectric.com.sg> wrote:

Depending on application:

Lincoln Electric 780 flux

Lincoln Electric P223 flux

Lincoln Electric 781 flux

Lincoln Electric SPX 80

Etc.


  From: "GERING, Erwin" [Erwin.GERING@airliquide.com]
  Sent: 03/05/2010 08:48 AM CET


  To: <materials-welding@googlegroups.com>
  Subject: [MW:4435] RE: 4421] Hispeed fluxes for SAW WELDING

 

Depending on application:

Oerlikon OP F55

Oerlikon Uniflux D1

Oerlikon OP 191

Etc…

 

With kind regards,

Erwin GERING

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens bcube bcube
Verzonden: donderdag 4 maart 2010 16:39
Aan: materials-welding@googlegroups.com
Onderwerp: [MW:4421] Hispeed fluxes for SAW WELDING

 

Dear all,

 

Can any one sent me the details releated to the Hi speed fluxes used for SAW welding .

 

 

Reg,

RBG

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...