Hello  sagar , 

So the valve has to be installed with respect to PPE not by flow direction ie. If the flow as per iso is east to west and when the valve is installed with respect to PPE the flow for valve is west to east and it doesn't matters ?? Is there a document or standard which gives detail explanation about PPE ???




On Mon, May 11, 2015 at 3:23 PM, sagar patil <sagar.tecnimont@gmail.com> wrote:
Orbit valves are single seated valves; this arrangement make the valves unidirectional.

Manufacturers of these valves mostly mark PPE on flange rims instead of flow directions.



On Thu, May 7, 2015 at 5:02 AM, TDK YOKESH <tdky167@gmail.com> wrote:
Warm Greetings folks ,

Being a welding/ material forum , I dont know whether I should be posting this .

What is PPE ( preffered Pressure End ) ??? How does it affect the flow ??? What if the flow direction and PPE  are different as per ISO?? how should the valve be installed . I mean with respect to PPE or flow direction ??? Please clarify . 

--

Best regards,

TDK YOKESH

QC INSPECTOR ( PIPING AND WELDING )

QUALITY CONTROL DEPARTMENT

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcQ7lSlmn1ExpyOpkX2RaZW-T5JttIFRfJMtPb23EzPZOQxDBU2w8PO-rDQ

Plot D1, Lumut Port Industrial Park,

Kg. Acheh, Mukim of Lumut,

Daerah Manjung, 32000 Sitiawan,

Perak Darul Ridzuan,

Malaysia

Tel No. : +601126527600

Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-TupYUac4gJpOfpFPtaE3CxW21Xn-nKesTc9QJLRN_jMTrw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAG38UkC-i6%3DNjuyGsLm7GAG1DBs7TBAizKs8tj7ao%2BMxQ9gRQ%40mail.gmail.com.

For more options, visit https://groups.google.com/d/optout.



--

Best regards,

TDK YOKESH

QC INSPECTOR ( PIPING AND WELDING )

QUALITY CONTROL DEPARTMENT

https://encrypted-tbn0.gstatic.com/images?q=tbn:ANd9GcQ7lSlmn1ExpyOpkX2RaZW-T5JttIFRfJMtPb23EzPZOQxDBU2w8PO-rDQ

Plot D1, Lumut Port Industrial Park,

Kg. Acheh, Mukim of Lumut,

Daerah Manjung, 32000 Sitiawan,

Perak Darul Ridzuan,

Malaysia

Tel No. : +601126527600

Email: tdky167@gmail.com

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKT-Tuo%2BScuYZ%3DKVAFfD-erwZ7Dzh8a%3DgG70vFnUwpz6fFy1rw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...