Dear Mr Hussain,

What kind type III or IV Crack? Could you explain these crack types?


On Sunday, September 28, 2014 4:04:55 PM UTC+7, engrshanas wrote:
Dear experts,
As per my expereince, we should use B9 instead of B3. During operation (One year) it will give type III or IV crack and we need to cut it out again. According to Babcock and Wilcox and Vallaourec & Mannesmann, it might give higher hardness and we may do not get the required micro structure as well. 

Kind regards
Muhammad Hussain
Lead Metallurgist
TCR Arabia Company Limited
Dammam- Saudi Arabia 



On Sunday, September 28, 2014 11:29 AM, Bala Nechur <bala....@phoenixindustrial.ca> wrote:


Hello Expert,
 
I recommend to use ER9S-B9 and E9018-B9 which will match the chemistry of A335 Gr P91 material.
 
Bala Nechur,
Corporate QA/QC Manager
Phoenix Industrial,
Office: 780-428-3130  Ext 736
Cell: 780-204-0239
Fax: 1-866-211-3193
Toll Free: 1-866-778-3130
PhoenixEmailSignaturew18001-01
                                                                                                     
The information transmitted is intended only for the addressee(s) and may contain confidential, proprietary and/or privileged material, unauthorized review, copying, distribution, taking of any action in reliance upon or disclosure is strictly prohibited. If you are not an intended addressee, please delete this message, including attachments immediately
 
Please don't print this e-mail unless you really need to. Copy of go green
 
From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of pras ari
Sent: September-26-14 10:16 PM
To: material...@googlegroups.com
Subject: [MW:22004] WELDING JOINT A335 P91
 
Dear Experts,

We have study case, on our project (steam power plant project), there was any welding joint i.e. welding pipe A335 P91 to A335 P91 with filler metal GTAW ER90S-B3 + SMAW E9015-B9 and PWHT 750 C with holding time 2 hours.
Please advise us, what impact these welding joint for strength and lifetime if compare with GTAW ER90S-B9 + SMAW E9015-B9 and PWHT 750 C with holding time 2 hours.
What can we do and the solution this case.

Thanks and regards
Winarko
QA/QC Welding Inspector
+6281288300094
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...