Dear Mohit,
 
F Number is an essential variable for welders qualification. If the F-No used in the CS does not cover that to be used for the Overlay as per QW-433, then the welder is not qualified to perform such overlay. In any case, you will also need to consider the requirement of QW-381.3.
 
Dear Mahendra,
 
When a chemical composition is stipulated in the WPS, it simple implies that every weld performed must meet the stipulated chemical composition and chemical analysis of the production weld may be required by spot check. It is then a requirement that every welder must be qualified using that particular WPS and strickly following the weld parameters as stipulated in the WPS.
 
Regards,
 
Rems Okonkwo
IWE Nigeria

On Fri, Sep 26, 2014 at 7:26 PM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear Sir,
Thanks for your reply.

Code is ASME section IX.and consumable is E309LMo.
My query is sir if a welder is qualified in CS Groove weld then how he can qualify for overlay as overlay is always done by Inconel or SS whatever it is!!

Best Regards,
Mohit Aggarwal.

On 26-Sep-2014 11:04 PM, "Rems Okonkwo" <rems.okonkwo@gmail.com> wrote:
Dear Mohit,
 
Although your query lack all necessary information like the applicable code, the type of consumable, materials etc but on a general note, welders qualified for clad restoration are not qualified to weld butt joints but when a welder is qualified on butt weld, the weld is qualified to weld clad restoration if only
 
1. requirement for Chemical composition.
 
2. within the F number of the consumable qualified,
 
3. within the welding position qualified
 
Please refer to ASME IX Art III (See Below)
 

QW-381.3 Alternative Qualification With Groove

Weld Tests.

When a chemical composition is not specified

in the WPS, welders or welding operators who successfully

complete a groove weld performance qualification

test meeting the corrosion

‐resistant overlay bend test requirements

of

QW-163 may be considered qualified for

corrosion

‐resistant overlay welding within the ranges defined

in

QW-350 or QW-360.
Regards,
 
Rems Okonkwo
IWE Nigeria
On Thu, Sep 25, 2014 at 3:43 PM, Mohit Aggarwal <aggarwalmohit05@gmail.com> wrote:

Dear Experts,

I have query regarding welder that if a welder is qualified for clad restoration overlay then he will be qualified to weld in groove joint or not.

If a welder is qualified for groove welding,then he will be qualified for clad restoration overlay or not.

Thanks!!

Best Regards,
Mohit Aggarwal.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...