Sunday, January 30, 2011

[MW:9559] diameter and thickness limit

Dear All,

My query is in regard to welder performance qualification diameter and thickness limit as per ASME Sec IX

As per QW 452.3, upper diameter limit is unlimited.

As per QW452.1b, for test coupon 13 mm and above, qualification limit is 'maximum to be welded.'

I would like to know that this "maximum to be welded" is to be considered same as unlimited or there is any limit.

With regards,

A.Husain


 

1 comment:

sudhan said...

TWO WELDERS QUALIFIED 6G POSITION IN 2 7/8" OD AND OVER WITH 14.2 MAXIMUM WELD METAL THICKNESS. CAN POSSIBLE TO ALLOW THESE WELDERS TO WELD 4" OD XXS THICKNESS (17.4 MM) AND COMPLETE THE JOINT.

[MW:35448] Hot tapping between piping and pipeline

Dear Expert we have hot tapping  from process piping b31.3 design  to cross country pipeline old pipe i think api 1104 design WPS that need ...