Hi,
In that case, you may change pipe groove to match J groove of fittings. It is easier than modifying a J groove to V groove.
regards,
LALU
On Thu, Mar 10, 2016 at 1:32 PM, Pradeep Chowdary <mechprady@gmail.com> wrote:
Sorry.. Typing mistake..--In Pipe Its V groove and in Fittings J groove ( its about the thickness 25mm)Pradeep
On Thursday, March 10, 2016 at 12:51:31 PM UTC+6, kannayeram gnanapandithan wrote:J in pipeTHANKS & BEST REGARDS,KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,CONSULTANT-WELDING & QUALITYOn Thu, Mar 10, 2016 at 11:54 AM, Pradeep Chowdary <mech...@gmail.com> wrote:Dear Experts,--I have an problem regarding with joint design, normally one end of pipe is came with V groove and fittings came with J groove, the thing is can we weld those joints..?? or we have to make J groove in pipe ?? Normally ASME 31.3 it's mentioned about thickness only. Apart from this, i remember that, Joint Desgin is a Non essential variable right??? So guys, shall i proceed for welding??Please help me out with this issue..Thanks and Regards,Pradeep
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a67b6d-b93d-47f0-9bf1-130c1f451684%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bb518a6f-69f4-43d4-83e6-53deaf1cb7e0%40googlegroups.com.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13uGmS2%2BF%3DLJcDiSOSPnZDwnY42DFd2Sa3nHuFJ6ViMhMQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment