Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP 
is a weathering structural steel 
It has better atmospheric corrosion resistance.
Use E 8018 - W1/W2  Electrodes

This is regularly  available in market 

Vishwas
IWE 
9823472273
Sent from my iPhone

On 20 Sep 2024, at 11:05 AM, sridhar cn <sridharcn305@gmail.com> wrote:


ER80S-Ni1(a nickel alloy filler wire), E81T1-Ni1C 9 (for FCAW process with 80 A+20 CO2) 
Please read it as "ER80S-Ni1(a nickel alloy filler wire), E81T1-Ni1C (for FCAW process with 
80 A+20 CO2)".
You can also try with E/ER309L which will help to avoid preheating or post weld cooing. But it 
is only an option.
Sridhar.


On Thu, 19 Sept 2024 at 19:27, sridhar cn <sridharcn305@gmail.com> wrote:
Mr.Xun Thong,
S355J2WP is a weathering steel.  E7018-1, E 8018-W2 (for higher strenths),
ER80S-Ni1(a nickel alloy filler wire), E81T1-Ni1C 9 (for FCAW process with 80 A+20 CO2) 
are generally suitable. 
Preheat & PWHT may be necessary to prevent cracking.
rgds,
Sridhar.

On Wed, 18 Sept 2024 at 21:22, Xuân Thông <xuanthong.hp@gmail.com> wrote:
Hi Experts,
Any one please give me the suggestion for welding consumables that will be used for S355J2WP.  If you have any WPS for this material, please let me know.
Thanks !

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHTP-O%3DA4OKzV%2B%3DRPnGBKXVW5o_q0B5dT60Ftz_xB%2BWJNqDf1w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYii2jJYt43s0RPm5xypt8tnEra_rkJC-f3iJXg7nAmEq3A%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...