Thursday, March 10, 2016

Re: [MW:24474] Joint Design

joint design is non essential that everybody knows, but in a joint , one member with J and another member with Bevel. This is not a good engineering practice to weld dissimilar bevel preparation???, in practical it is difficult

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Thu, Mar 10, 2016 at 3:05 PM, anand gupta <gupta_0576@yahoo.co.in> wrote:
Please check asme sex ix that joint design is non essential so can weld.

a p gupta
saudi
aramco

Sent from Yahoo Mail on Android


From:"Pradeep Chowdary" <mechprady@gmail.com>
Date:Thu, 10 Mar, 2016 at 9:45 AM
Subject:[MW:24457] Joint Design

Dear Experts,

I have an problem regarding with joint design, normally one end of pipe is came with V groove and fittings came with J groove, the thing is can we weld those joints..?? or we have to make J groove in pipe ?? Normally ASME 31.3 it's mentioned about thickness only. Apart from this, i remember that, Joint Desgin is a Non essential variable right??? So guys, shall i proceed for welding??

Please help me out with this issue..

Thanks and Regards,

Pradeep

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a67b6d-b93d-47f0-9bf1-130c1f451684%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1457602532.75616.YahooMailAndroidMobile%40web192703.mail.sg3.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eP4TpvfOzYBm%3DCUdgJbcptOcB4zQ4eQp1rxBspxiLW0Zw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...