You should work to a consistent set of standards for any part of a project (piping, structure, vessels, ship structures, nuclear plant etc), and if you fail to do that, should anything go wrong later you could end up with difficulties explaining what you have done or why you have done it, possibly in court. You need to look at your contract with your client, and the specification references therein. If you are not compliant you need to raise a concession request and get their approval. If they are reliant on you for technical expertise then keep it consistent to minimise your liabilities.

 

Alan Denney

AKD Materials Consulting Ltd

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Narender reddy
Sent: 10 March 2016 06:55
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24459] structural welding NDE Accaptence

 

Dear experts

 

We have an ITP for structural welding in that WPS & PQR prepared as per ASME SEC IX.

  1. NDE acceptance is mentioned as ASME B 31.3 which is related process piping.

my question is 

  1. Can we use AWS D 1.1 as acceptance criteria?.
  2. Can we two different types of codes in same ITP.such like that ?

 

regards

Narender reddy.M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c5adff87-f633-476c-98d5-4015c40fec19%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...