Re: [MW:24440] Acceptance for bottom plate of storage tank (API 650)


There is no requirement in API 650 for flatness of bottom plates.
Sent from my iPhone

On 22-Feb-2016, at 12:48 pm, Vishal Sharma <vishalsharma.sharma225@gmail.com> wrote:

Dear Experts,

We found 42 mm distortion in bottom plate after welding with shell. Is it acceptable? Please share reference standard. 
Please note tank fabrication is going on within shop.

Br,
Vishal Sharma

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAK1segupjbGRtScdgV3DhDP4k-7sx2y_NjnfcBC8fovg-g6ag%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...