Mr.bala murugan,
you are giving the wrong reference, this statement is not mentioned in the api 650, please clarify your reference,
On Thursday, March 3, 2016 at 3:25:33 PM UTC+3, bala murugan wrote:
Dear Friend,
As per API 650, Cls 7.5 it was mention in dimension tolerance topic
that The bulging of bottom plate shall not exceed .25% of dia of tank
(for tank dia <40m) unless otherwise mentioned. 100mm max. for tank
dia >40m.
Thanks,
Bala
On 2/22/16, Vishal Sharma <vishalsharm...@gmail.com > wrote:
> Dear Experts,
>
> We found 42 mm distortion in bottom plate after welding with shell. Is it
> acceptable? Please share reference standard.
> Please note tank fabrication is going on within shop.
>
> Br,
> Vishal Sharma
>
> --
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-weld...@googlegroups.com .
> To post to this group, send email to material...@googlegroups.com .
> Visit this group at https://groups.google.com/group/materials-welding .
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/ .CAAK1segupjbGRtScdgV3DhDP4k- 7sx2y_NjnfcBC8fovg-g6ag% 40mail.gmail.com
> For more options, visit https://groups.google.com/d/optout .
>
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1019f078-7dca-47b1-ad68-63c0941bed0c%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment