It is pipe joint right?
Then the full circonférence must undergo pwht

Sent from my BlackBerry 10 smartphone.
From: 'Agustin Jimenez' via Materials & Welding
Sent: Σάββατο, 5 Μαρτίου 2016 - 05:58
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: RE: [MW:24433] Requirement of PWHT after repair in P91 after SR

Hi.
It Is not necessary to do full joint PWHT, only 1" is necessary PWHT.

Agustin




Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: 'Ramesh Barot' via Materials & Welding <materials-welding@googlegroups.com>
Fecha:04/03/2016 07:04 AM (GMT-04:30)
Para: Materials Welding <materials-welding@googlegroups.com>
Cc:
Asunto: [MW:24432] Requirement of PWHT after repair in P91 after SR

Dear Experts,

Please give your opinion if 30 inch joint found repair material p91 after SR in only one inch.


Is it necessary to do full joint PWHT??

If a joint getting pwht again then what effects might be on joint and material??


Thanks

Ramesh Barot


Sent from my LG Mobile

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000f4242.02933e1c1d5502b1%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/qy6w6fdn0fmqpf1qs852cd7e.1457126245598%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

2 comments:

Unknown said...

Dear All,

What ever , repair is must under go once again PWHT, Since it's P91 materiel. My suggestion, after repair done it should be go for HEAT TREATMENT.

Please refer Sec.1 under Repair Section.

Thank you

Unknown said...

Dear All,

It's mandatory that after repair attend it should go for PWHT 100%. Since the Material is P15F and there is no more violation regarding this.

Any further classification, Please refer Section 1 under Repair and reweld

Agustin,

Please confirm that, in which section sates that only repair portion has to go PWHT??

Help me out with this

Thank you

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...