Saturday, March 5, 2016

Re: [MW:24436] Welder Qualification as per ASME SEC IX

Dear Mr. Mohd. Azam,

please refer QW 322.1 for expiration of qualification and 322.2 for renewal of qualification.
For your case qualification has expired as per 322.1(a) and re qualification should be done as per 322.2 (a).

Regards,

Anosh Wankhade






From: Naskabir Vengassery <naskabir@gmail.com>
Sent: Fri, 04 Mar 2016 12:27:26
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:24429] Welder Qualification as per ASME SEC IX
Dear Azam,
in my opinion considering only ASME Sec IX,
1) if you are confident on the Welder's skill , you can take advantage of ASME Sec IX:2013, QW-322.2 by arranging a test using each processes that he was previously qualified. only process is important. material, shape, thickness, positions and electrical or other parameters are not restricted. After visual you can go for RT in lieu of Bend test. This will revalidate all his previous qualification with the same PROCESS(s).
2) if the welders ability is under doubt or he was not successful in (1) above, retests for all his previous qualifications has to be carried out (QW-322.2(b))

 

On Sunday, December 27, 2015 at 5:31:54 PM UTC+3, Azam Mohd wrote:

Dear Expert,

"X" welder working with company and left the organization. Again after Two or three year he is joining back same company. All earlier certificate is available with company with proper documentation.

 

Is it possible to renew his earlier certificate with one sample based on RT or visual inspection OR All new qualification is to be done New. Qualification code is ASME SEC IX.

 

Pls provide your valuable input with standard reference.

 

Thanks & Regards,

Mohd. Azam

Doha-Qatar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ca1d318-947d-42d3-9b41-6da261d36965%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Get your own FREE website, FREE domain & FREE mobile app with Company email.  
Know More >

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1457074646.S.11149.7018.f4-235-241.1457158443.31487%40webmail.rediffmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...