Dear Yokesh,

Code doesn't suggest NDE on Orifice Flange. It's depend upon the client, here we face the same issue and we done with PT that too 10% .

If anything lemme know..

Pradeep 

On Thursday, February 25, 2016 at 9:41:20 AM UTC+6, Tdk Yokesh wrote:
Good morning folks ,

Does code suggest NDE ( MPI or PT ) to be carried out once the root of the orifice flange is flush grinded .



Sent from my Mi phone

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a0e45850-a62e-45c4-be6b-807ec8efce6f%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...