Skip to main content

Re: [MW:5294] DIN Wire IQI Thickness

Wire IQI
Used to assess sensitivity ; quality of technique 
Pl refer DIN 54109 (1962); ISO 1027
Wire set 1-7; set 6-12; set 10-16 (1,7,6,12,10,16 represent wire numbers)
3 sets - each set having 7 wires (overlapping with adj set) arranged in GP
usually 2% or lesser value of sensitivity is required for general applications
Smaller no 1% indicates higher sensitivity -critical applications

wire dia          wire No
   mm                        
   3.2 ...............  1 
   2.5  ............... 2
   2.0  ............... 3
   1.6   ...............4
   1.25 ...............5
   1.0   ...............6
    0.8  ...............7
---------------------------    
    1.0   ..............6
    0.8  ...............7  
    0.63 ...............8
    0.50................9
    0.40..............10
     0.32..............11
    0.25...............12
-----------------------------
    0.40..............10
    0.32..............11
    0.25..............12
    0.20 .............13
    0.15 .............14  
    0.125............15
    0.10 .............16
  ---------------------------


Regds
MSR
--------------------------------------------------------------------------------------
On Sun, May 30, 2010 at 12:20 PM, Srinivas Engr <srinivas.gmsrini@gmail.com> wrote:
Dear All

Where to we find DIN wire IQI Thickness?
Which standard is deals about DIN wire IQI Thickness?
Where to refer?

--------------------------------------------------------------------------------------------------------------------------------------

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .