Re: [MW:5201] NDT after PWHT

Dear Friends,
We need to check all requirements in line with code specific to the item . Certain codes do specify NDT after PWHT . Certain client specifications specify the NDT requirements after PWHT . so do not conclude  requirements  in general.You may refer this in BS 5500 for pressure vessels or B31.3 for piping

 Regards,


----- Original Message -----
From: dlsltd@telus.net
To: materials-welding@googlegroups.com
Sent: Thu, 20 May 2010 23:41:40 +0530 (IST)
Subject: Re: [MW:5199] NDT after PWHT








 

 

I don't believe there is any requirements, but
on  P5-B materials, it is a common practice as cracks have been known
to form after 24 hours on these materials. I have heard of some materials
on "Hold" pending another RT after the initial test after 7 Days.

 

I have just completed PWHT on ASME 1 piping and
there is no requirement on P1 material for additional RT after cool
down.


----- Original Message -----



Sent: Thursday, May 20, 2010 6:30
AM

Subject: [MW:5198] NDT after PWHT








Dear friends

We just finished PWHT in an LPG sphere acording to ASME VIII
section I, and I can´t find in the code the part that obligues to Xray
after this treatment, any one has experience with this? where does
ASME VIII say it has to be done?

Thank you

Luis AlbanƩs

 

--
To post to this group, send email to materials-welding@googlegroups.com
To
unsubscribe from this group, send email to
materials-welding-unsubscribe@googlegroups.com
For more options, visit this
group's bolg at http://materials-welding.blogspot.com/
The
views expressed/exchnaged in this group are members personel views and meant
for educational purposes only, Users must take their own decisions w.r.t.
applicable code/standard/contract documents.




--

To post to this group, send email to materials-welding@googlegroups.com

To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com

For more options, visit this group's bolg at http://materials-welding.blogspot.com/

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Click for exclusive coverage on the New Bajaj Pulsar 220 the fastest Indian bike

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

[MW:30043] Weep hole

If weep hole is not provided in dummy pipe before welding What will happen??? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/da251ee6-fa7f-4851-b876-cdb3834ae341%40googlegroups.com .