Dear Sir,

please find the Index for your kind referance

On Fri, Dec 22, 2017 at 12:34 PM, Mani kandan r <manikandanr21@gmail.com> wrote:
Dear sir,

can anyone send pipeline pressure drop calculation due to temp change......

Thanks in advance

Regards,

R.Manikandan


On Dec 22, 2017 9:41 AM, "'PRAMODH NAIR' via Materials & Welding" <materials-welding@googlegroups.com> wrote:
Pradeep,

For pipeline, refer the below sample (Minimum Requirement)

1.       Pipeline Hydrostatic test diagram

2.       Pipeline schematic diagram and P&ID

3.       Pipeline alignment sheet/ ISO drawing

4.       Line list

5.       Pipe book and tie in weld

6.       Welded sections map (pipe line)

7.       Pre-test critical component removal and test preparation

8.       Punch list

Released for cleaning

9.       Pipeline cleaning inspection

Released for Gauging

10.   Pipe Gauging inspection

Released for filling and flooding

11.   Water analysis report

12.   Pipeline flooding &filling inspection

Released for hydro test

13.   Temperature record (temperature and pressure for stabilization)

14.   Pipeline pressure /volume log(for 50% test pressure)

15.   Air content calculation report

16.   Pressure/temperature log (for100% test pressure)

17.   Pressure/temperature log (for pressure holding)

18.   Pipeline hydrostatic test report

19.   Pipeline dewatering report

20.   Pipeline post test critical components reinstatement

21.   Caliper pigging

22.   Pipeline swabbing check

23.   Pipe drying report

Released for Purging

24.   Final Package Acceptance (Singing of Sub-con/Contractor/Client)



Thanks with warm regards,

Pramodh M.R


If We Work With Determination And Perfection, Success Will Follow



On Friday, December 22, 2017, 9:17:26 AM GMT+3, Sajeev P <sajeevlaxmi@gmail.com> wrote:


Hi Pradeep,

Please refer attached Document.

Regards,
Sajeev P.

On Thu, Dec 21, 2017 at 8:06 AM, Pradeep kumar hormis <pkhormis@gmail.com> wrote:
Sirs

Could anyone can give me a sample copy of pipeline Hydrotest package index (contents).

Thanks & Regards

PRADEEPKUMAR HORMIS

Mob: +966-58 16 20 710



 
 


 

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--



Best Regards,

Joydev Dalai
Dy. Manager - QA/QC
+91-7260898902
JHPL Project,
Kalpataru Power Transmission ltd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...