Thursday, March 10, 2016

Re: [MW:24468] Temporary Blind plate thickness

As a bolted flat head

Sent from my BlackBerry 10 smartphone.
From: pradip kumar Sil
Sent: Πέμπτη, 10 Μαρτίου 2016 - 08:33
To: materials-welding
Reply To: materials-welding@googlegroups.com
Subject: [MW:24456] Temporary Blind plate thickness

Dear All,
Can anyboby give idea during hydrotest " How we will calculate temporary blind plate thickness for a certain pressure i.e. 40 bar "
Regards,

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8keHPrixTW0ZsphcZbjJdfu7bH%3Dd1mogsXsnpXw2jwW%3DQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...