Dear Sir,

 

Indeed ASME B 31.3 is related to process piping but ASME section IX is related to Boiler en Pressure Vessels, so in this case for structural welding I would say full project (also PQR's / WPS) should be executed according to AWS D1.1.

 

If you can/may use different codes mixed up is depending on your customer requirements, if he allows it than it would be acceptable. I personally prefer to keep things clear and follow only one specification in order to prevent any discussions.

 

For NDT AWS D1.1 has his own acceptance criteria but for NDT techniques AWS is referring to ASME V, so there you already have a mix-up allowed by applicable specification.

 

Met vriendelijke groeten / Best Regards,

 

Herman Pieper

QA-QC Inspector / CSWIP + IWI-C Welding Inspector / IWT / Materials Expert

 

Job van der Havestraat 6

8384 DB, Wilhelminaoord

Cell: +31 6 51691215

 

Van: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Namens Narender reddy
Verzonden: donderdag 10 maart 2016 07:55
Aan: Materials & Welding
Onderwerp: [MW:24459] structural welding NDE Accaptence

 

Dear experts

 

We have an ITP for structural welding in that WPS & PQR prepared as per ASME SEC IX.

  1. NDE acceptance is mentioned as ASME B 31.3 which is related process piping.

my question is 

  1. Can we use AWS D 1.1 as acceptance criteria?.
  2. Can we two different types of codes in same ITP.such like that ?

 

regards

Narender reddy.M

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c5adff87-f633-476c-98d5-4015c40fec19%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...