Pradeep,
Normally Weld Bevels are made for below reasons
1. Accessibility (of torch & electrodes)
2. Flowability of the Weld Metal
3. Thermal conductivity of Base Materials ( where thickness also is considered when it changes the flow from 2D to 3D)
As per ASME Sec.IX, joint detail is a non-essential variable and if the above criteria are taken care of welding pipe with V bevel will not have any effect provided you produce sound weld joint without any lack of side wall fusion.
Thanks & Regards
J.Gerald Jayakumar
0091-9344954677
From: Pradeep Chowdary <mechprady@gmail.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Thursday, March 10, 2016 11:54 AM
Subject: [MW:24457] Joint Design
Dear Experts,
-- I have an problem regarding with joint design, normally one end of pipe is came with V groove and fittings came with J groove, the thing is can we weld those joints..?? or we have to make J groove in pipe ?? Normally ASME 31.3 it's mentioned about thickness only. Apart from this, i remember that, Joint Desgin is a Non essential variable right??? So guys, shall i proceed for welding??
Please help me out with this issue..
Thanks and Regards,
Pradeep
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a67b6d-b93d-47f0-9bf1-130c1f451684%40googlegroups.com?utm_medium=email&utm_source=footer.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment