Re: [MW:24442] PWHT Requirment for overlay (Inconel 825 on SA 352 Gr LCC)

For overlay my suggestion would be to use IN 625 (ER Ni Cr Mo- 3) instead of 825 wire. Pwht of CS. Vanchi

On 7 Mar 2016 12:39 p.m., "Brajendra Singh" <brajendra1020@gmail.com> wrote:
Dear Experts,

We are going to qualify an weld overlay procedure with Inconel-825 (ERNiFeCr-1) on SA352 Gr LCC with following variables.

1.Base Metal Thickness- 40 mm
2.Qualification Std- ASME Sec IX
3.our actual job thickness ranging from 50 to 100 mm.
4. Deposit overlay thickness is 5 mm.
5. Welding Process-Manual GTAW

Kindly advice for following queries.

1. PWHT required or not- please suggest with code reference & what will be the effect if PWHT not been done.
2. PWHT Temperature & time requirement.

Regards,

Brajendra S Patel

MOB: +91 7057406907




--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ade8fd07-fd08-487d-910f-8bd6ec2894c1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B6Tn1JtFFeMm5EykMxgsK3yQJ3LbpmkbY67ATQa7XeKnu8riQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...