Saturday, March 5, 2016

RE: [MW:24433] Requirement of PWHT after repair in P91 after SR

Hi.
It Is not necessary to do full joint PWHT, only 1" is necessary PWHT.

Agustin




Enviado desde mi smartphone Samsung Galaxy.


-------- Mensaje original --------
De: 'Ramesh Barot' via Materials & Welding <materials-welding@googlegroups.com>
Fecha:04/03/2016 07:04 AM (GMT-04:30)
Para: Materials Welding <materials-welding@googlegroups.com>
Cc:
Asunto: [MW:24432] Requirement of PWHT after repair in P91 after SR

Dear Experts,

Please give your opinion if 30 inch joint found repair material p91 after SR in only one inch.


Is it necessary to do full joint PWHT??

If a joint getting pwht again then what effects might be on joint and material??


Thanks

Ramesh Barot


Sent from my LG Mobile

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...