Removing galvanizing:
Try using 50% dilute HCl, dip your part in it till the bubbling stops, then wash off / rub off with baking soda.
Vinegar also is useful.
But take care not to inhale fumes.
BR,
Shashank C Vagal
From: Perumal Govindan <perumalgovindan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Friday, 4 March 2016 7:56 AM
Subject: Re: [MW:24429] Re: How to protect Serration of Flanges during Hot dip galvanization
Hi
I am forgetting the cheminal name, which will be applied on the serrated surface before HDG bath, once done it will be cleaned to recover the serration.
I am forgetting the cheminal name, which will be applied on the serrated surface before HDG bath, once done it will be cleaned to recover the serration.
Requested to contact the HDG agencies for more details.
With kind regards
Govindan
Kuwait
Govindan
Kuwait
On 11 Feb 2016 07:00, "Hamid Jabbari" <lifebod@gmail.com> wrote:
-- Does any one know how could i remove the hot galvanized coating from face of flange?--
plz advise
On Monday, August 23, 2010 at 1:08:56 PM UTC+4:30, aly mhaskar wrote:
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/75d1da68-c97b-4709-b526-afb7cfd25136%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANiuf9ezuZ21SrWWWCy-jg6M4q5HRtC8h4FopYjcp5mscRMMyw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments: