Re: [MW:24416] PWHT

We consider 80% aggregate time and temp.
As per qw-407.2 of qualify procedure.

On Mar 1, 2016 2:59 PM, "Maulik Thakkar" <mlkthakkar2@gmail.com> wrote:

Dear all,
I have two queries:
MOC: P8Gr1(SS347 internal)
PWHT on job with LAS is at 705+/-10 degree C for 10 hrs.
Available PQR: 700 degree C for 8 hrs.
Can I support same PQR for welding of SS347 internal which will undergo PWHT at 705+/- 10 degree C along with LAS???

Impact: not applicable for SS.

Second query:
Interpretation of QW407.1 (b).

Regards,
Maulik

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUMCrJL9dRmq0Q%3DDEJpfNmP%3DJ%3DRmrTk4fzV7cjfUj7FKdw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANykCaThRuP1tdHJKc6oFnUkX4pAxu1RuQAjmq%2BzrDbQV%3Dhxkg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...