Re: [MW:24416] PWHT

what is grade of LAS?, u can if it is P22

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Mon, Feb 29, 2016 at 8:38 PM, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:

Dear all,
I have two queries:
MOC: P8Gr1(SS347 internal)
PWHT on job with LAS is at 705+/-10 degree C for 10 hrs.
Available PQR: 700 degree C for 8 hrs.
Can I support same PQR for welding of SS347 internal which will undergo PWHT at 705+/- 10 degree C along with LAS???

Impact: not applicable for SS.

Second query:
Interpretation of QW407.1 (b).

Regards,
Maulik

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUMCrJL9dRmq0Q%3DDEJpfNmP%3DJ%3DRmrTk4fzV7cjfUj7FKdw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMcd06_MMJe4cuG2hWXtiLf3H%2Bj5F%3D1KfBHympE7qw63w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35597] INCONEL 825

Dear all  INCONEL 825 matching filler   ER NI FECR-1 its correct please guide me Regarding  Elavarasan -- https://materials-weldin...