Skip to main content

RE: [MW:7958] No of Welders

Dears,

Is it acceptable to qualify 2 welders (ASME IX - 6G - one by side) per cupon (down from 12" NPS) or not ?

In my opinion, technically it is not acceptable to qualify two welders in same cupon

1. As per Section IX , diameter is specified for welder qualification QW 452.3. 

2.Since hand movement will be different in two sides (clock wise and anti clock wise), each welder is preferred to qualified in separate coupons. If the thickness does not matters ( low thickness) , you can qualify the welders with 2" pipe. Also record wise ( RT films), it will be difficult.

I am no so familiar with API 1104

thanks and regards,

Arun




From: alexis_viteri@hotmail.com
To: materials-welding@googlegroups.com
Subject: RE: [MW:7949] No of Welders
Date: Sat, 30 Oct 2010 12:27:53 -0500

Dear Members,
 
Is it acceptable to qualify 2 welders (API 1104 - 6G - one by side) per cupon (down from 8" NPS) or not ?
Is it acceptable to qualify 2 welders (ASME IX - 6G - one by side) per cupon (down from 12" NPS) or not ?
 
Thank and regards
 

Date: Sat, 30 Oct 2010 10:37:56 +0000
To: materials-welding@googlegroups.com
Subject: Re: Re: [MW:7943] No of Welders
From: drpaulosejohn@rediffmail.com

Dear Mr. Arun,

Minimum number of welders to be qualified by one WPS is - One welder. The welder who performs the PQR coupen welding is automatically becomes qualified. Please refer 2nd para of QW 301.2 of Section IX:2010 and para 621 of API 1104:2007.

Regards,
Dr. Paulose John
QA/QC Manager,
Unisis Engineering,
Saudi Arabia
.
On Sat, 30 Oct 2010 14:15:07 , No ID Specified wrote
To my knowledge there is no limit for number of welder qualification  upon one WPS, You can qualify as many as per to the requirement for your project. 
 
 
 
Here By,
 
P.BalajiRajan,
-------Original Message-------
 
From: Arun Das
Date: 10/28/10 17:39:52
Subject: [MW:7911] No of Welders
 
Sir,
 
Minimum number of welders to be qualified upon one WPS is mentioned in SEC 1X or API 1104.
We are using PIPE,16"X0.375"WT STD SCH API 5L X52
 
Thanks in advance
 
with regards,
 
Arun S Das

 
FREE Animations for your email - by IncrediMail! Click Here!
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...