Skip to main content

Re: [MW:7902] Welder Performance Qualification ASME IX

Heat Input = AXVX1000/60Xspeed= MM/SEC with clamp meter
regards
Sujay

On Thu, Oct 28, 2010 at 8:52 AM, masoom ghole <masoomghole@gmail.com> wrote:
how to consider current and voltage range according to pqr in wps
according to asme sec ix

On 10/27/10, (PBR)P.BalajiRajan <pbalajirajan@gmail.com> wrote:
> Mr Larry,
>  As per to the ASME IX
> QW-423   Alternate Base Materials for Welder
>               Qualification
> QW-423.1 Base metal used for welder qualification
> May be substituted for the metal specified in the WPS in
> Accordance with the following table. When a base metal
> Shown in the left column is used for welder qualification,
> The welder is qualified to weld all combinations of base
> Metals shown in the right column, including unassigned
> Metals of similar chemical composition to these metals.
> Base Metals for Welder                                  Qualified Production
> Qualification                                                   Base Metals
> P-No. 1 through P-No. 15F,                             P-No. 1 through P-No.
> 15F,
> P-No. 34, and P-No. 41                                   P-No. 34, and P-No.
> 41
> Through P-No. 49                                            through P-No. 49
> P-No. 21 through P-No. 26                              P-No. 21 through P-No
>  26
> P-No. 51 through P-No. 53 or                          P-No. 51 through P-No.
> 53 and
> P-No. 61 and P-No. 62                                   P-No. 61 and P-No.
> 62
>
> QW-452.3
> GROOVE-WELD DIAMETER LIMITS
> Outside Diameter                             Outside Diameter Qualified, in.
> (mm)
> Of Test Coupon, in. (mm)                              Min.
> Max.
> Less than 1 (25)                                  Size welded
> Unlimited
> 1 (25) to 27⁄8 (73)                                 1 (25)
>   Unlimited
> Over 27⁄8 (73)                                      27⁄8 (73)
>  Unlimited
>
> GENERAL NOTES:
> (a) Type and number of tests required shall be in accordance with
> QW-452.1.
> (b) 27⁄8 in. (73 mm) O.D. Is the equivalent of NPS 21⁄2 (DN 65).
>
>
> Here By,
>
> P.BalajiRajan,
> Inspection Engineer,
> Velosi Certification LLC,
> P.O 3408 Doha-Qatar.
> Mobile- Qatar +97433120091,
>              India  +919842659329.
>
>
>
>
>
> -------Original Message-------
>
> From: Larry
> Date: 10/27/2010 11:22:50 AM
> To: materials-welding@googlegroups.com
> Subject: [MW:7839] Welder Performance Qualification ASME IX
>
> Hi There,
>
> We have qualified a welder on an ASME IX WPS with the following:
>
> Position: 6G
> Size: 100NB
> Specs: A333- WPL6 (P1, G1)
> Process: GMAW/FCAW (F-No.: 6 electrode)
>
> As per QW-423.1 and QW-433, will the welder be qualified to weld the
> following for production?
>
> Position: as required
> Size: All practical diameter and plate
> Specs: A106B (P1, G1), SA 312-316L (P8, G1)
> Process: GTAW (F-No.: 6 electrode)
>
>
> Thank you in advance.
>
>
> Cheers,
>
> Larry
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...