J in pipe
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
On Thu, Mar 10, 2016 at 11:54 AM, Pradeep Chowdary <mechprady@gmail.com> wrote:
Dear Experts,--I have an problem regarding with joint design, normally one end of pipe is came with V groove and fittings came with J groove, the thing is can we weld those joints..?? or we have to make J groove in pipe ?? Normally ASME 31.3 it's mentioned about thickness only. Apart from this, i remember that, Joint Desgin is a Non essential variable right??? So guys, shall i proceed for welding??Please help me out with this issue..Thanks and Regards,Pradeep
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/a1a67b6d-b93d-47f0-9bf1-130c1f451684%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOrbdEsUiuBcX%3DNP%2BsXxOZi16YtxRy9o4b7JRF6ZVuS0Q%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
1 comment:
Sorry typing error.. Pipe in V groove and Fittings came in J grrove..