Tuesday, March 8, 2016

Re: [MW:24444] IGC AFTER PWHT

if it is client requirement ,yes, otherwise not required

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY

On Mon, Mar 7, 2016 at 10:18 PM, Maulik Thakkar <mlkthakkar2@gmail.com> wrote:

Dear experts,

Is it require to have IGC testing in PQR if representatives seam undergoes in PWHT.

If yes then pls provide the reference.
MOC: SS347
COC: ASME SEC VIII DIV1

Regards,
Maulik

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFK0MUPuJ_ES%3D-9KhHCMEN28JQ8EuJiYVewkxQdURqSmYe0oww%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMA7o1__QzepJA_V5UDzUmD-TTVmyOELBytcpAwAio-5g%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...